I've walked into a lot of shops over the years, and there's one thing I see over and over again. The press gets all the attention. New squeegees, new pallets, more pressure, slower stroke, another flash. Meanwhile, the screens coming out of the screen room have never been measured once.
Here's the thing I tell every crew I train: it's screen printing, not press printing. The press just pushes ink through the screen. The screen is what actually prints your shirt. And two of the biggest things that decide how that screen performs are your emulsion over mesh (EOM) and your exposure.
Most shops either skip measuring these completely or give them a quick glance and move on. I get it. It's not the fun part. But if you're fighting your prints on press every day, there's a really good chance the problem started back in the screen room.
EOM: your stencil gasket
EOM is how much emulsion is built up on the print side of the screen, past the thickness of the mesh itself. That extra layer is your stencil gasket. It's what seals against the shirt during the stroke and gives the ink a clean wall to sit inside of.
When that gasket is right, you get:
- Sharper edges and cleaner halftones
- More consistent ink deposit from screen to screen
- Better opacity without cranking up squeegee pressure
- Less sawtoothing and less ink bleeding out from under the stencil
When it's too thin, there's nothing to seal against the garment. Printers start compensating with more pressure, harder strokes and extra passes, and now you're wearing out your arms, your rubber and your screens to fix something that should've been handled at the coating trough. Too thick and you'll fight detail, longer exposures and ink that doesn't want to clear.
How to measure it
Grab a thickness gauge and take two readings: the bare mesh, then the coated and dried screen. Keep the same units the whole time.
EOM % = (coated thickness − bare mesh) ÷ coated thickness × 100
Your target will shift a little depending on your emulsion type (diazo, dual-cure or photopolymer, and how high its solids content is), but for most apparel work we like to see somewhere around 15–25%. Take readings in a few spots across the image area, not just one corner. Once you find a coating method that lands you in range, write it down — emulsion type, trough edge, number of coats on each side — and make it the standard for that mesh count.
I just saw this at a shop last week. Their 158 mesh screens were coming in under target, and the press crew had been chasing ink deposit for months. Adjusting the coating did more for them than any squeegee change could have.

Exposure: lock it in
You can nail your EOM and still lose the screen if it isn't exposed right. Exposure is what turns that emulsion into a durable, fully cured stencil.
Underexposed screens are the sneaky ones. The emulsion is soft on the squeegee side, so it feels slimy when you wash out, breaks down halfway through a run, pinholes, and can be a nightmare to reclaim. A lot of "bad emulsion" complaints are really underexposed screens.
Overexposed screens hold up fine, but you lose your detail. Fine lines and small halftone dots close up because light creeps under the film edges.
The fix isn't guessing or going off "what we've always done." Run an exposure test with a Stouffer scale on a screen coated to your standard EOM. Tape it to your film, expose, wash out, and read which step held. Each step lets through less light than the one before it, so you can see exactly where the emulsion is fully cured and where it isn't. Adjust your time until you're landing on the step your emulsion manufacturer recommends, and make sure your detail is still holding. Then it goes on the chart right next to your coating standard.
EOM and exposure go hand in hand. Change one and you need to recheck the other. A thicker stencil needs more light to cure all the way through.
Measure it, then keep measuring it
Testing once and calling it good isn't enough. Things drift. Retest your EOM and exposure whenever:
- You bring in a new mesh count
- You switch emulsion brands or products
- Your exposure unit gets new bulbs or gets moved
- Humidity in the screen room changes with the seasons
- New people start coating screens
Keep a simple log by the coating station with mesh count, EOM reading, exposure time and who coated it. Spot-check a few screens every week. It takes a couple minutes, and it'll save you hours of troubleshooting on press.
You don't need a ton of gear to get started. A thickness gauge, a Stouffer scale, a hygrometer for the screen room and a loupe to check your detail will cover most of it.

Learn more at Impressions Long Beach
Want more tips like this? Come see us at Impressions Long Beach. MADE Laboratory is running the education at the show this year, so you'll find us leading sessions on the stuff that actually moves the needle in your shop: screen room fundamentals, press setup, ink systems, workflow and more.
Until then, go grab a gauge and measure a few screens. You might be surprised by what you find. Remember: it's screen printing, not press printing.